Quote:
Originally Posted by WheelMan

Well......if I don't feel dumb
Was thinking Ti would have great wear resistance.  I'm assuming the drive pins in the ends that go into the drive cups are what wear so quickly?
I'm not gonna be able to get myself to run these now. Looks like I'll be on the hunt for a steel set. I keep seeing people mention the Stainless UE CV's, but I've never actually seen any?...are these even more rare than the Ti ones?
-Travis
|
The drive pins can be changed if they wear out although i believe they are steel even on titanium cvds. The area that wears fastest is the area where the barrel goes in.
The stainless were the old version before Robin at ue found that the black oxide steel was actually better and last longer.